Sunday, June 2, 2013

Re: [MW:17869] Deposited weld metals

QW 451 - t refer to weld metal deposit.


On Sun, Jun 2, 2013 at 9:49 AM, Michael Lawrence Arokiasamy <mila.welding@gmail.com> wrote:
Dear All,
Please clarify my doubt in WPS as per ASME SECTION IX 
Process:  GTAW + SMAW
PQR base metal Thickness:  10.31 mm
WPS Base metal thickness range:  5.0-19.0 mm
Deposited weld metal:  GTAW (5mm)+ SMAW (14mm)
How I can find out the weld metal thickness GTAW 5mm & SMAW 20.62mm
(I saw the section IX, QW-404.30 & QW-450 Table also but I can't understand)

Thank you,
 
Regards,
A.Michael Lawrence
Welding Inspector

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:35346] Cast-iron welding

Any advice for cast iron welding Sent from Yahoo Mail for iPhone