Saturday, February 2, 2013

[MW:16669] Minimum Puff piece in piping

Dear Experts,

    I have used 150mm of puff piece in the spool of 34'' pipe as per the drawing but my QA Dept. tells that in piping we can't use 150mm of puff piece and they have suggested me to use a minimum of puff piece of the OD of the pipe id i.e. a length of 850mm.

Please give me the section on which the puff piece details is  mentioned in the ASME section.

With Regards,

SANTOSH KUMAR NAYAK

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...