Dear Mr.LP
-- As I understanding that ..
WPB Means .. Wrought Pipe Which is made from Weldable Pipe ,Grade B .Plz go through ASTM A 234 ,You can get % of Corbon details with respect to different grades .
Suresh
--
On Thu, May 3, 2012 at 9:33 AM, LOKNATH PATRA <loknathpatra26@gmail.com> wrote:
Dear experts,
can anyone tell me for cs fittings material we use A234 Gr WPB.what is the full form of WPB & what is the carbon % in it.& other than that what grade can we use for cs fittings.
Regards
--
L.P
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Thanks & Best Regards,
Suresh
Mobile No: 974 - 5 5 4 3 1 7 8 8 / 7 7 1 3 4 5 9 0 . ( Qatar )
Suresh
Mobile No: 974 - 5 5 4 3 1 7 8 8 / 7 7 1 3 4 5 9 0 . ( Qatar )
91 - 92 92 905 905 ( India )
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/