Re: [MW:13492] Pre-heating for cutting

Hi,
No Need to do for cutting.
 
Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
German-Thai Boiler Engineering Cooperation Limited.
Rayong Factory ;
379 Moo.6 Soi 8, Tambol Pananikom,
Nikompattana, Rayong 21180 THAILAND
Tel : +66 38 897 035-9 Ext. 137
Fax : +66 38 897 034
Hand Phone: 0066 892512282


From: jesti fer <jesti_fer@yahoo.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Monday, January 16, 2012 4:52 PM
Subject: [MW:13484] Pre-heating for cutting

Dear Experts,
 
I need your help for this subject, We are fabricating some piping as per B31.3, the material ASTM A106 Gr.B, 8"Sch-XXS and 160 and we are doing preheat and PWHT for welding, but my enquiry pre heat is required for cutting also? It is mentioned in any code or any other were? Please help me
 
Jesti
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...