Dear,
We have material API 5L X70 , 30” O.D ; Thk. 13.33mm , we are planning to do PQR using ER 80S-Ni1(mod) 2.4mm for GTAW and E8018-C3H4R – Bohler welding consumable. Is it correct?
Please advice.
Thanks
Mohamed
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...