Monday, December 19, 2011

[MW:13230] regarding thickness qualification as per ASME sec-IX

Dear Experts,

Is there any provision for thickness qualification as per sec-IX while
doing heat treatment in upper Transformation range?

As per clause no-407.4 in Sec-IX, it indicates that if ur test piece
receives heat treatment in upper transformation range then the thk
qualificatin reduces to 1.1 times of thk instead of 2T.

I want to know that i want qualification of 2T instead of 1.1T while
doing HT in upper transformation range.

Kindly give ur opinion for that

Is there any provision for thk qualification for this, so i can get 2T
Qualification while doing HT in upper transformation range.

Regards,

Ankit Khatri

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...