Sunday, August 28, 2011

Re: [MW:12320] type 3 joint

Pls. refer UW12 . If type 3 joint is less than 24"Dia, efficiency can not be increased by RT
Regards,
Sasi

On Thu, Aug 25, 2011 at 7:21 PM, imran khan <imransian@gmail.com> wrote:
Dear Experts,
 
I need your urgent attention please
 
As per UW-12
 
Type 1........... both side welded butt joint(full radiography) ...........efficiency 1
Type 3............single vee but welded joints(no radiography)...........efficiency 0.60
 
my question is can i use type 3 joint as type 1 to get higher efficiency say 1.0 if the joint is 100% radiographed.
--
With Best Wishes,
 
Imran Khan
 
Cell:+966580790536
   

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...