Dear All
We usually use E6010 for welding Low Alloy galvanized carbon steel pipes (SMAW welding)
Regards
SAMI
--- On Thu, 8/25/11, Vikram Bhat <kvikrambhat@gmail.com> wrote:

From: Vikram Bhat <kvikrambhat@gmail.com>
Subject: Re: [MW:12307] Filler wire for galvanized
To: materials-welding@googlegroups.com
Date: Thursday, August 25, 2011, 5:56 PM

Gents,
 
Usually cellulose electrodes are being used in order to get the better penetration of the zinc.

On Thu, Aug 25, 2011 at 2:54 PM, naveed ahmed <naveed_aytb@yahoo.com> wrote:
can any body clarify
which filler wire is required for welding galvanized pipe ?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...