dear ,

It is difficult to weld galvanized pipe , first you have to grind the
ends of the pipe to be welded , you can use E70S3 for carbon steel
galvanized pipe ,when zinc burn off it produce smoke, it can cause
health risk.

On Thu, Aug 25, 2011 at 4:24 PM, naveed ahmed <naveed_aytb@yahoo.com> wrote:
> can any body clarify
> which filler wire is required for welding galvanized pipe ?
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...