Mr Samir,
The shell side and tube side pressures are 37/39 kg/cm2
Temperature on shell side in/out: 246/120 deg C
Tube side in/out: 101/229 deg C
This exchanger is a U-tube bundle exchanger
Thickness of tube sheet is 210 mm,1290 OD, weight: 1490 kgs
Thickness of channel flange: 190mm
Thickness channel bonnet:  36/32
Weight of channel bonnet is 1820 kgs.
regards


From: "SAMIR THAKKAR" <prabhasteel.samir@rediffmail.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Date: 08/17/2011 12:57 PM
Subject: Re: [MW:12246] ASTM A 193 Gr B7 to B16





Mr.Prasad,
may i know what is the pressure in HE.??? AND what is the thickness of CH. cover ???

SAMIR THAKKAR
(PRABHA STEEL IND.)


From: M S R K S Prasad <MSRKSPrasad@nagarjunagroup.com>
Sent: Sat, 13 Aug 2011 16:53:57
To: materials-welding@googlegroups.com
Subject: [MW:12205] ASTM A 193 Gr B7 to B16

Dear members,

I am thinking of changing MOC of one of the exchanger channel cover bolts from B7 to B16 as the exchanger channel cover is leaking very frequently. Whenever it leaks we tighten it manually the leak minimizes after few days it
resurfaces.In each tightening  the nuts are moving by about 10 to 15 deg.

I request members to suggest whether the choice of B16 is OK are any other bolting material is better than B16 is available.

with regards

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Treat yourself at a restaurant, spa, resort and much more with
Rediff Deal ho jaye!

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...