Here is a screenshot of the API-recommended consumables for mismatched materials concerning Copper and Nickel based alloys.  The reference document is API RP 582 Annex A Table A.4 .
 
Darcy Morin


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of MAHANTESH LONI
Sent: Friday, August 19, 2011 6:04 AM
To: materials-welding@googlegroups.com
Subject: [MW:12277] WELDING SA516 GR70 to INCONEL 600

Dear All
 
Pl pass on procedure to weld SA 516 Gr70 to Inconel 600. Otherwise atleast some litrature on this would be helpful.
 
Thanks & Regards
Loni

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...