Subject: [MW:12273] FW: 11108] DUPLEX S.S. (S.S. 2205) TO AUSTENITIC S.S. (Grade 316L) welding.
U can use E2209 or E309MoL
Ahmed Osman
Sr Q.C. Eng.
-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of CHINTUKUMAR GANDHI
Sent: Saturday, May 21, 2011 12:21 PM
To: materials-welding@googlegroups.com
Subject: [MW:11108] DUPLEX S.S. (S.S. 2205) TO AUSTENITIC S.S. (Grade 316L) welding.
Dear Experts,
I come across with very strange welding combination. That is Duplex stainless steel to ausatenitic steel welding. Here Flange is SS 316 L & pipe is duplex stainless steel (2205).
plz guide me abt which filler wire I should use? & which good engineering practises should adopt during welding.
Chintu Gandhi
Welding Engineer
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Friday, August 19, 2011
RE: [MW:12278] FW: 11108] DUPLEX S.S. (S.S. 2205) TO AUSTENITIC S.S. (Grade 316L) welding.
Here is the chart from API which deals with SS mismatches.
Darcy Morin
Subscribe to:
Post Comments (Atom)
[MW:35692]
Dear all Can I do MPI above painting surface for cs tank Regards, Sriram Srinivasan -- https://materials-welding.blog...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment