Friday, August 19, 2011

Re: [MW:12275] Difference between SB625 UNS NO8904 & SA 240 Type 904L

Dear Kapil,
The uns N08904 is introdused in those two standards are the same (SA240 TP904L and SB625 UNS N08904), but just in chemical and mechanical properties. There is too much restrictions in SB625 other than chemical and mechanical properties. If had a look on SB625 and it had some requirements for dimennsional and tolerances of products which theu are not mentioned in SA240.
 
Regards
On Fri, Aug 19, 2011 at 9:14 AM, kapil bhamburdekar <kapilbhamburdekar@gmail.com> wrote:
Dear All Experts,
 
I want to know about the Difference between ASME SB625 UNS NO8904 & ASME SA 240 Type 904L,
 
I have checked chemical and physical properties which are same for both, but still Inspector is demanding for SB 625 Plate instead of ASME SA 240 Type 304 plate.
 
Regards,
 
Kapil Bhamburdekar
QA Engineer

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
M.Shokri Arfaei
International Welding Engineer
RT, UT ASNT Level III
ERI-Metallurgy Lab. Manager
Tel: +98 21 66283693
Fax: +98 21 66283693
Mob.: +98 912 139 4023
Web: www.metallurgylab.com

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...