Surface Roughness Produced by Different Manufacturing Process

Knowing what manufacturing process can produce surface finishes that desired on a surface can be an added advantage while making the designs. Here is a table showing maximum and minimum Ra values can produced on each production methods.  
 

Process

Roughness Average, Ra – Micrometers μm

Maximum

Minimum

Flame Cutting

25

12.5

Snagging

25

6.3

Sawing

25

1.6

Planing, Shaping

12.5

1.6

Drilling

6.3

1.6

Chemical Milling

6.3

1.6

Elect. Discharge Machining

4.75

1.6

Milling

6.3

0.8

Broaching

3.2

0.8

Reaming

3.2

0.8

Electron Beam

6.3

0.8

Laser

6.3

0.8

Electro-Chemical

3.2

0.2

Boring, Turning

6.3

0.4

Barrel Finishing

0.8

0.2

Electrolytic Grinding

0.6

0.2

Roller Burnishing

0.4

0.2

Grinding

1.6

0.1

Honing

0.8

0.1

Electro-Polish

0.8

0.1

Polishing

0.4

0.1

Lapping

0.4

0.5

Super Finishing

0.2

0.025

Sand Casting

25

12.5

Hot Rolling

25

12.5

Forging

12.5

3.2

Perm. Mold Casting

3.2

1.6

Investment Casting

3.2

1.6

Extruding

3.2

0.8

Cold Rolling, Drawing

3.2

0.8

Die Casting

1.6

0.8

Above high and low values are typical for each production methods. But values other than high and low Ra can be obtained under special conditions for each process.

Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Fri, 8/19/11, vaibhav Joshi <vnjoshi.leo@gmail.com> wrote:

From: vaibhav Joshi <vnjoshi.leo@gmail.com>
Subject: [MW:12270] Material processing and Surface Finish in Ra
To: materials-welding@googlegroups.com
Date: Friday, August 19, 2011, 12:57 PM

Dear all,

can any one tell me avg surface roughness value in Ra with respect to material processing ( Grinding ,Machining, etc) ?

Regards,
Vaibhav Joshi


     rr
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...