Re: [MW:12257] NDE Personnel Qualification As per ASME B31.3

Hi,
NDE Level I/II shall be qualified by the qualified Level-III person (Inhouse or External Training Institute) with the written paractice as per ASNT-SNT-TC1A. Normally most of them are certified by the Training institue with Level-III persons.

Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Wed, 8/17/11, Vikram <kvikrambhat@gmail.com> wrote:

From: Vikram <kvikrambhat@gmail.com>
Subject: [MW:12252] NDE Personnel Qualification As per ASME B31.3
To: "Materials & Welding" <materials-welding@googlegroups.com>
Date: Wednesday, August 17, 2011, 10:07 PM

For NDE Personnel Qualification As per ASME B31.3 is it Mandatory to
Certify the NDE Personnel by Employer as per SNTC-SNTC-1A or Who are
qualified in NDE Level - II in the method from external Levle - III
will be sufficient.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...