Welder Performance Qualification References

 

QW-452.1(b) - THICKNESS OF WELD METAL QUALIFIED

QW-452.3 - GROOVE-WELD DIAMETER LIMITS

QW-452.4 - SMALL DIAMETER FILLET-WELD TEST

QW-452.5 - FILLET-WELD TEST

QW-452.6 - FILLET QUALIFICATION BY GROOVE-WELD TESTS

QW-461.9 - PERFORMANCE QUALIFICATION — POSITION AND DIAMETER LIMITATIONS

(Within the Other Limitations of QW-303)



 
Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Wed, 8/17/11, John Henning <jhenning@deltak.com> wrote:

From: John Henning <jhenning@deltak.com>
Subject: [MW:12250] RE: 12249] W.Q.P. Ranges
To: materials-welding@googlegroups.com
Date: Wednesday, August 17, 2011, 10:39 PM

Regarding base metal thickness, the welder is not restricted as to how thick the base metal is.  He is only restricted as to the thickness of deposit he can make.  This is addressed in Intrepretation IX-77-19

 

Deposited weld thickness qualified is given in QW-452.1(b).

 

It is takes a  little to get there, but ultimately, for welders:   

·         Pipe diameter limits are given in QW-452.3 for performance qualification test on pipe

·         And per QW-461.9 for performance qualification test on plate

 

Hope this answers your question

 

John

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of john clough
Sent: Wednesday, August 17, 2011 5:55 AM
To: materials-welding
Subject: [MW:12249] W.Q.P. Ranges
Importance: High

 

Sirs
Does anyboby have referance regarding Diameter and thickness ranges for welder qualification tests for ASME Section1X.
 
John

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...