Re: [MW:12235] Material Test Certificate Clarification / EN 10.204:2006 / Urgent Attn

Hi,
UNE EN10204:2006 is a spanish standard and EN10204:2004 and UNE EN10204:2006 are same.
 
Thanks & Regards,
 
(Karthik)

On Tue, Aug 16, 2011 at 2:12 PM, Vino Varghese <vinopvarghese@gmail.com> wrote:
Dear All,
 
We have recieved Structural Material Certificate, S 355 JR + AR from CELSA Barcelona.
The Certification refers to UNE EN 10.204:2006.
 
I know only Certification of Material as per EN 10204:2004.
 
Can anyone share some detail with regard to UNE EN 10.204:2006.
Whether UNE EN 10.204:2006 is same as EN 10204:2004?
 
Hope to see as usual co-operation from all end.
 
Thanks & Regards
Vino P Varghese
Doha-Qatar

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...