[MW:12250] RE: 12249] W.Q.P. Ranges

Regarding base metal thickness, the welder is not restricted as to how thick the base metal is.  He is only restricted as to the thickness of deposit he can make.  This is addressed in Intrepretation IX-77-19

 

Deposited weld thickness qualified is given in QW-452.1(b).

 

It is takes a  little to get there, but ultimately, for welders:   

·         Pipe diameter limits are given in QW-452.3 for performance qualification test on pipe

·         And per QW-461.9 for performance qualification test on plate

 

Hope this answers your question

 

John

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of john clough
Sent: Wednesday, August 17, 2011 5:55 AM
To: materials-welding
Subject: [MW:12249] W.Q.P. Ranges
Importance: High

 

Sirs
Does anyboby have referance regarding Diameter and thickness ranges for welder qualification tests for ASME Section1X.
 
John

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...