Wednesday, March 16, 2011

Re: [MW:10381] filler for SS to Inconal welding

Dear Mr Kataria
NiCrFe3 or Ni CrMo3 both
are compatable to use for welding SS to Inconel
However some time for higher service temp. and resistance to pitting corrosion  NiCrMo3 is prefered and for that matter some time consultanant insist for NiCrMo3
Regards
Hegde

From: Vinod Kataria <vinod.kataria@blissanand.com>
To: materials-welding@googlegroups.com
Sent: Wed, 16 March, 2011 11:11:02 AM
Subject: [MW:10379] filler for SS to Inconal welding

Dear All,
I need to weld SS-316 to Inconal 825 as per API 582 (table attached) the
filler should be ErNiCrFe3 but I wants to use ErNiCrMo3 can anyone provide
me some authentic documents so that I can use ErNiCrMo3.
Regards
Vinod Kataria
GM-Operation
Bliss Anand Group.
+91-9560199004.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...