Re: [MW:10357] bolts and nuts material

Dear Ahmed Eissa, this is stainless steel bolt identification. It is stamped on bolt head.

Sincerely,

Mustafa YAPAR
=====================

iPhone'umdan gönderildi.

15 Mar 2011 tarihinde 08:52 saatinde, Ahmed Eissa <ahmedeissa16@yahoo.com> şunları yazdı:

dear all
 
what is this material stamped on bolts and nuts mean ( A2-70 )   ????
 
Which code or standard??
 
it is not in A193 &A194
 
thanks

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...