Mr illangkumaran,
                           Coating is the basic process; painting is one method of coating. 
Types of coatings:
1. Heat resistant coatings
2. corrosion resistant
3. Performance
4. Aesthetic coatings
5. MEMS
6. Application coatings
and many more
Now coming to painting, it is a method of coating to protect the substrate by means of oil based, acrylic based, water mainly for corrosion resistance.
2011/3/15 S. Waheedullah Shah <waheedullah@fatima-group.com>

According to my perception coating is a deposition process which is achieved mostly by ionic deposition e.g chrome plating and painting is application by mechanical process e.g by brush, painting gun etc.

 

Syed Waheedullah Shah

Unit Manager Inspection

Pakarab Fertilizers

Multan

Tel. Office: +92-61-90613098

Mob.: +92-333-3829925

            +92-300-2221535

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of k.ilangkumaran ilangkumaran
Sent: Tuesday, March 15, 2011 9:49 AM
To: materials-welding@googlegroups.com
Subject: [MW:10349] painting&coating

 

Dear experts,

 

                   Can anybody explain me differences between coating and painting?

 

 

Regards

Ilangkumaran

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
regards,
Harish.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...