Dear friend,
As per API450 . Bottom plate inspection is as decided by you & bottom plate to vertical shell connection by LPI & Chalk-Kerosine leak test.
vikas sahu 

On Fri, Mar 11, 2011 at 5:59 PM, srinu p <sree.dream6@gmail.com> wrote:
Dear All,
 We have two existing tanks ( 20 years old) 3 mtrs height and 5.7 mtrs dia.. Bottom plate thickness - 8 mm.
 
As per client requirement we have shift the tanks to another place and also they want to change the Bottom plate.
1. As per API standard  or any other standards, if we change the bottom plate, which type tests are required for bottom plate inspection. My opinion is Vaccum Box and DPI or MPI tests are enough? or Any other tests are required?
2.And also if we are using  same bottom plate UT thickness guage checking and VB, DPI/MPI tests are enough? Is it acceptable?
 
Please share your experience.
 
regards,
 
P.Srinu
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...