Re: [MW:10273] Mechanical Testing of A36 25 mm ThK Plate 3G FCAW Process, As per AWS D1.1. for WPS Qualification, Impact is required or not?

Hi

No requirement for the CVN tests for the A36 material

Thanks & Regards,

K. Babu

----- Original Message -----
From: "Srinivas Engr" <srinivas.gmsrini@gmail.com>
To: "Materials & Welding" <materials-welding@googlegroups.com>
Sent: Thursday, March 10, 2011 11:54 PM
Subject: [MW:10268] Mechanical Testing of A36 25 mm ThK Plate 3G FCAW
Process, As per AWS D1.1. for WPS Qualification, Impact is required or not?


> Dear All,
>
> As per AWS D1.1,
> Base material - A36,
> 25mm Thk Pl,
> FCAW process,
> E71T1 - Filler material
> 3G position.
>
> From table 4.2 says tensile & bend test is enough.
> But I get heared from one great testing Labratory tat Imapct test is
> also required?
> Pl confirm me about this WPS, wat are the test need for WPS
> qualification.
> Experts pl comment on above..
> Those having qualified WPS of above welcome to comment..
>
> Regards
> Srinivas
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...