Re: [MW:10249] PWHT after pipe spool repair

Normally u need to NDT, Hardness test and check the weld integrity by pressure test. 

On Wed, Mar 9, 2011 at 10:33 AM, <vnbhatt@gmail.com> wrote:
We have a seam less carbon steel SA-106 pipe spool duly Post weld heat treated.
Due to mis match, we had to cut two circumferencial welds and re done them. We are ready to conduct PWHT again, the question is do we need to re test any property of spool or place a test pipe and check properties again?

Thanks all!!
Sent on my BlackBerry® from Vodafone

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
 

Best Regards,

K.V.S.Reddy,
Q.C.Inspector(Piping&Welding),
BS-132 Project,
SKEC Eng& Con Ltd.,
Postbox no-55653,
Sabahiya-54567,
Kuwait.
kvsreddy777@gmail.com,karryswamireddy@yahoo.com,
Ph:00965-94414396.
PleaseSave a tree. Don't print this e-mail unless it's really necessary

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...