Tuesday, March 8, 2011

Re: [MW:10226] normalizing temperature range for CS materials

Dear,
The Normalizing temperature is usually taken to be 920 degree C (or
the tempereature above upper critical temp. line in iron carbon
diagram). Also there is no reference for normalizing temperature range
mentioned in the asme.

Regards,
Qamar

On 3/7/11, krishna <wiqw@rediffmail.com> wrote:
> dear
> all,&nbsp;&nbsp;&nbsp;&nbsp;&nbsp;&nbsp;&nbsp;&nbsp;&nbsp;&nbsp;&nbsp;&nbsp;&nbsp;&nbsp;&nbsp;&nbsp;&nbsp;
> what is the normalizing temperature for carbon steel?whether asme codes
> specifies the temperature ranges if so pls mention the referencethnkxkrishna
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...