Re: [MW:10199] normalizing temperature range for CS materials

Normally it is 910degC. It depends on the chemical composition and you can plot it in Fe-C equilibrium diagram above AC3 temperature point.

J.GERALD JAYAKUMAR
00919344954677
 


--- On Mon, 3/7/11, iacob catalin <cataliniacob2000@yahoo.com> wrote:

From: iacob catalin <cataliniacob2000@yahoo.com>
Subject: Re: [MW:10193] normalizing temperature range for CS materials
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Date: Monday, March 7, 2011, 8:36 AM

it's in function from class cs steel;in general is 800 grd C-----900grd C

From: krishna <wiqw@rediffmail.com>
To: materialswelding <materials-welding@googlegroups.com>
Cc:
Sent: Monday, March 7, 2011 10:04 AM
Subject: [MW:10192] normalizing temperature range for CS materials

dear all,
                  what is the normalizing temperature for carbon steel?
whether asme codes specifies the temperature ranges if so pls mention the reference
thnkx
krishna

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...