Re: [MW:10187] Tungsten inclusion appeared in WQT

Hi,
Pls.Refer QW191.2.1 (b) - Tungsten inclusion are included in Rounded Indications.
Tungsten inclusion acceptance criteria shall be as per QW191.2.2 (b)

QW191.2.1
(b) Rounded Indications. Porosity and inclusions such
as slag or tungsten are represented on the radiograph as
rounded indications with a length three times the width or
less. These indications may be circular, elliptical, or irregular
in shape; may have tails; and may vary in density.

Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Mon, 3/7/11, k.ilangkumaran ilangkumaran <k.ilangkumaran@yahoo.com> wrote:

From: k.ilangkumaran ilangkumaran <k.ilangkumaran@yahoo.com>
Subject: [MW:10184] Tungsten inclusion appeared in WQT
To: materials-welding@googlegroups.com
Cc: rajandt1@yahoo.com
Date: Monday, March 7, 2011, 11:30 AM

Dear experts,
 
                As far I know that slag inclusion allowed 3mm size as per secIX section QW-191.2.2(2)(b). Tungsten inclusion is not accepted kindly advise me if i am wrong.
 
Regards
Ilan
                  

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...