Sunday, March 6, 2011

Re: [MW:10180] Combination of GTAW & SMAW PQR for a WPS.

no,
pl read qw 200.4

On Sun, Mar 6, 2011 at 11:57 AM, Srinivas Engr <srinivas.gmsrini@gmail.com> wrote:
Dear All,

As per ASME sec 9
PQR 1 - GTAW T - 7.11mm , 1.5 to 14.22mm - A106 Gr.B

PQR 2 - SMAW T - 12.70mm, 5 to 25.4mm - A 106 Gr.B

No PWHT & No toughness.

My doubt is,1)  is it possible to combine the above WPS to make GTAW &
SMAW combination.?
If possible wats thickness range.?

2) & Regardless of WPS,
My welder is qualified with Tig Process & Arc Process in seprately,
Is it possible to put them in production for Same A106gr.b material in
combination like Tig root & Arc Filler.
If it not possible. Pl tell me para which restricts this.


Regards
Srinivas

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...