RE: [MW:10147] Can I use E 7018 in Pipe root runs? What's the disadvantages?

Mr. Srinivasan

E-7018 is universally accepted low hydrogen electrode, helping many welding engineer and welders to produce quality welds. However for pipeline welding , especially for root passes, this electrode has some limitations. In our electric utility we do not perform a lot of cross country pipeline welding. But there're some such pipelines for  carrying natural gases, to fire in the boilers.Field welding  and desired quality of such piping's may not be easy always.

There're some practical welding issues with E-7018 for root passes, e.g less digging arc, which may cause inconsistent root penetration, greater slag volume  and less friable slag, which is  sometimes difficult to move. Generally our experiences is with E-7010 root +E-7018 filling passes.

The attached product of Bohler looks promising. Feel free to dig up more information and I'm sure some members from BTW would be more than happy to help you further in your queries.

Thanks.


Pradip Goswami,P.Eng.IWE
Welding & Metallurgical Specialist & Consultant
Ontario,Canada.
Email-pgoswami@sympatico.ca,
pgoswami@quickclic.net

-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of James, GeraldJayakumar
Sent: Wednesday, March 02, 2011 4:33 AM
To: materials-welding@googlegroups.com
Subject: RE: [MW:10104] Can I use E 7018 in Pipe root runs? Wats the disadvantages?

I suppose it requires highly skilled welders to get uniform root penetration which could pass Radiography testing. For Piping it is normal practice to use GTAW for the Root Run & Next pass, & for remaining passes joint can be completed using SMAW E7018

-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Engineer Mech
Sent: Wednesday, March 02, 2011 2:22 PM
To: Materials & Welding
Subject: [MW:10087] Can I use E 7018 in Pipe root runs? Wats the disadvantages?

Hi All,

Can I use E 7018 in Pipe root runs? Wats the disadvantages?
Can i go E 7018 root run& filler WPS qualification?

Regards
Srinivasan

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchanged in this group are members personnel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

**********************************************************************
Confidentiality Notice

This communication and the information it contains:-
(a) Is intended for the person(s) or organization(s) named above and for no other person(s) or organization(s). 
(b) May be confidential, legally privileged and protected in law. Unauthorized use, copying or disclosure of any of it may be unlawful. If you have received this communication in error, please contact us immediately by email at Postmaster@fwuk.fwc.com.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchanged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...