Thursday, March 3, 2011

RE: [MW:10118] welding of ASTM A240 type 409 S40900 steel plate

ER/E409Nb , generally used in automobile industry, Only GMAW/FCAW wire could be available in the market.

 

S40900 (Type 409) has been replaced by S40910, S40920, and S40930. Unless otherwise specified in the ordering information, an order specifying S40900 or Type 409 shall be satisfied by any one of S40910, S40920, or S40930 at the option of the seller. Material meeting the requirements of S40910, S40920, or S40930, may at the option of the manufacturer be certified as S40900

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Martin Prad
Sent: Thursday, March 03, 2011 4:09 PM
To: materials-welding@googlegroups.com
Subject: [MW:10116] welding of ASTM A240 type 409 S40900 steel plate

 

Hi,
 
Could you please advise which consumable/wire can be used for welding of this type of steel?
 
regards,
Martin.


No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...