Wednesday, March 16, 2011

[MW:10390] WQT

Dear experts,
 
              Good day for all. While qualifying performance qualification for the welder with
3F and 4F fillet welds, I had noticed lot of undercuts and poor weld profile so I have rejected 4F piece. But 3F weld somewhat ok and its accepted.
 
I have to qualify this welder as per section IX. As far as performance qualification is concerned if the one piece is failed the entire qualification test is failed.But our contractor insist me to accept 3F. Should I reject both pieces or reject only one which is failed.
 
Kindly someone correct me if i am wrong and if possibel refer the para in section IX or from
QW-300 of section IX.
 
Thanks and regards
Raja K

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...