Sunday, March 13, 2011

[MW:10305] Re: CS to SS welding

For welding CS to SS it is good to use ER309L.

Distortion is less produce in TIG welding, but it is very slow
process. So depend upon your job requirement you have to choose the
process.

On Mar 10, 3:18 am, praveen nair <praveen_nair9...@yahoo.co.in> wrote:
> dear experts,
>
>    we have to make a rectangular type of furnace, in that we have to weld SS304 bars into CS plate from both sides and chances of distortion is more, plate thickness comes around 16mm and bars of 10 mm, client requirement in MIG or TIG welding,
> which process is better MIG or TIG to reduce distortion...??
> Can i use ER308 filler wire..?
> and methods for reducing distortion. We are doing stitch welding mainly
>
> praveen nair

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...