Thursday, March 10, 2011

[MW:10258] WELDED FITTINGS WITH TWO SEAM WELD

Dear all,


We ordered welded Carbon Steel & Stainless Steel fittings (45 & 90 degrees ELBOW, TEE, REDUCER … ) according to ASTM A234 and ASTM A403, but the manufacturer offered welded type with  two seam for above 12" & 16" for Stainless Steel and Carbon Steel respectively.

According to ASTM A234, ASTM A403 and ASTM A960, I have not seen anything related to number of seam weld.

Now my questions are :


1-In which specification or Standard has been specified that welded fittings should be one seam or two seam weld?

2-Whether welded Fittings with two seam are acceptable or not ? if yes, under which condition?

 

Kind Regards,


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...