[MW:10130] Minimum length for RT examination for PQR & WPS? ASME Sec 9?

Dear all,

As per QW 302.2, minimum length required for qualification of welder
or welding opeator by RT is 6 inch /150mm length.

My question is it same for PQR & WPS qualification.?

Regards
Srinivas

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step