can anybody explain "how to prepare WPS for CS(A106 Gr.B for example) or SS(A304) , which codes we have to refer in ASME sec ix?
take the material thickness range 3.6mm to 10mm
 
 
thanks,
shankar.k
qc inspector
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step