Please read ASME sec IX, QW 200.2.f page 15, 2010 edition. Multiple
WPS or Multiple PQR can support any defined PQR or WPS. Also check
essential variables of QW 256.
regards, ( conclusion : as long as the same parameters ,procedures
used it can qualify for plate also automatically. no need to make a
separate WPS or PQR ! )
WPS or Multiple PQR can support any defined PQR or WPS. Also check
essential variables of QW 256.
regards, ( conclusion : as long as the same parameters ,procedures
used it can qualify for plate also automatically. no need to make a
separate WPS or PQR ! )
Mohan
On Feb 28, 1:44 pm, Zakaria ghrab <zakaria.gh...@gmail.com> wrote:
> Hi all,
>
> I have GTAW/SMAW PQR, i need use to qualify SMAW plate WPS, think it's
> possible only for Fillet weld. i'm right ?
>
> --
> GHRAB Zakaria
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments