Monday, June 21, 2010

Re: [MW:5685] stroge tank API 650


Dear  Ramesh,
 
We have been faced same problem in our previous project.I agreed with you that API 650 does not stated clearly about bottom plates distortion.
 
In best my knowledge we need to minimize the distortion as much as we can during welding.I strongly recommended you to use low heat input and use good condition automatic welding machine.
 
Thanks
 
Suresh
 
QA/QC Specialist
On 6/21/10, Ramesh <ram2ram_2000@yahoo.com> wrote:
Dear all,
can any one explain storage tank bottom plate thermal distoration due to welding as per API 650 how we get the tolernce of expect peaking, banding,plumpness,and other.only bottom plate waveness tolerence not shown extally.

 
 
 
 

Thanks and Best Regards,

 Balakrishnan Ramesh

QA/QC Dept

QA/QC Inspector.Tanks/Silos

Daelim Saudi Arabia Co.Ltd

Value Creating Global Plant Builder

 SAUDI KAYAN HDPE PROJECT

8 ram2ram_2000@yahoo.com

      jayak@daelim.co.kr

 (KSA #-+966530647157

 

 
 
 
 


--- On Mon, 6/21/10, KASHKOUSHA <kashkousha1@yahoo.com> wrote:

From: KASHKOUSHA <kashkousha1@yahoo.com>
Subject: Re: [MW:5682] weld SA-106 to 9 Cr materials P No 5B gr 1 or gr 2
To: materials-welding@googlegroups.com
Date: Monday, June 21, 2010, 12:45 PM

dear ahmed
yes,by using ER 90S-B9(GTAW)&E9018-B9 (SMAW) or E 9015-B9
the joint should be heat treated acc .to ASME B31.3

 
H.KASHKOUSHA

 


From: Ahmed Hafez <diesel2002@hotmail.com>
To: Welding Material <materials-welding@googlegroups.com>
Sent: Mon, June 21, 2010 1:42:17 PM
Subject: [MW:5681] weld SA-106 to 9 Cr materials P No 5B gr 1 or gr 2

good morning every one
is it applicable to weld SA-106 to 9 Cr materials P No 5B gr 1 or gr 2
 
thanks and best regard


Your E-mail and More On-the-Go. Get Windows Live Hotmail Free. Sign up now.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks  & Best Regards,

Suresh

Mobile No: 91-92 92 905 905

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...