Re: [MW:5490] Active TIG?

there is a Non essential variable in QW 256 called flux (see QW 404.50 in ASME IX)

Dr. G. Dilintas - Authorized Inspector Supervisor
I&F Regional Technical Manager
Bureau Veritas Piraeus - Greece
Tel: +30 210 40 63 113/4
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04
Inactive hide details for pankaj abhang <pankaj.abhang1@gmail.com>pankaj abhang <pankaj.abhang1@gmail.com>


          pankaj abhang <pankaj.abhang1@gmail.com>
          Sent by: materials-welding@googlegroups.com

          09/06/2010 13:10

          Please respond to
          materials-welding@googlegroups.com

To

materials-welding@googlegroups.com

cc


Subject

Re: [MW:5486] Active TIG?

Ref


 
Dear kesavalunanda,
 
 Active-TIG welding ( hereinafter called as A-TIG welding ) is a welding method capable of drastically increasing further its penetration depth than in the conventional TIG welding by applying an active flux on the surface of steel product placed on the welding line. This welding method was proposed in 1960's, and is practically applied so that it can be easily used by the progress of recent research and development. By this, a drastic efficiency improvement can be materialized in TlG welding, drawing remarkable attention to it. which is such a new welding method.welding.
 
 
 
Regards,
 
Pankaj
On Mon, Jun 7, 2010 at 8:42 PM, kesavalunanda <kesavalunanda@yahoo.co.in> wrote:
      Dear Friends,
       
      Can  anybody clarify my doubt….please,

       

      the  question is" what is A –TIG (Active-TIG) ?"

       

      This question is  asked in AMIIW(Associate  membership in Indian Institute of Welding-kolkata-www.iiwindia.com) Exam-Summer-2009(AME-15)

       

      Thanks,

      Regards,

       K.NANDAGOPAL ;

      +91 9698997022

      +91 9360049258-

      Tamilnadu,

      INDIA

       

       

      --
      To post to this group, send email to
      materials-welding@googlegroups.com
      To unsubscribe from this group, send email to
      materials-welding-unsubscribe@googlegroups.com
      For more options, visit this group's bolg at
      http://materials-welding.blogspot.com/
      The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...