Wednesday, June 9, 2010

Re: [MW:5489] RE: 5484] Range of Pressure gauge to be used

Please check ASTM E 1003:2005 clause 8.1. the pressure gauges range shall be Minimum 1.5 to maximum 4 times the maximum test pressure.
 


 
On Wed, Jun 9, 2010 at 2:48 PM, Praveen Kumar <praveenkumar.sek@gmail.com> wrote:

       Normal Operating Pressure be confined to 25-75%  of the scale.
       Refer attachment
 
       The system of Test Pressure falls in 35 % to 65%  of gauge scale range.pressure gauge
       dial shall be min of 150mm. this is for as per EIL spec.
 
 
Regds,
 
Praveen Kumar
 

 
On Wed, Jun 9, 2010 at 3:16 PM, V.K.N. Umasankar <umasankar.vkn@gmail.com> wrote:

Normally accepted norms are 25% to 75%

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Bathula Anil Kumar
Sent: 08 June 2010 17:16
To: materials-welding@googlegroups.com
Subject: [MW:5484] Range of Pressure gauge to be used

 

Dear Friends,

 

Can any let me know what is the maximum and the Minimum limit of the pressure gauge that can be used for testing , is there any code governing this

 

Thanks and Regards,

Bathula Anil Kumar

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Regards,

S.Tulasi Ramu
+971 50 8175303 ( Abudhabi), +91 9866998074(India).

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...