Re: [MW:5488] RE: 5484] Range of Pressure gauge to be used


       Normal Operating Pressure be confined to 25-75%  of the scale.
       Refer attachment
 
       The system of Test Pressure falls in 35 % to 65%  of gauge scale range.pressure gauge
       dial shall be min of 150mm. this is for as per EIL spec.
 
 
Regds,
 
Praveen Kumar
 

 
On Wed, Jun 9, 2010 at 3:16 PM, V.K.N. Umasankar <umasankar.vkn@gmail.com> wrote:

Normally accepted norms are 25% to 75%

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Bathula Anil Kumar
Sent: 08 June 2010 17:16
To: materials-welding@googlegroups.com
Subject: [MW:5484] Range of Pressure gauge to be used

 

Dear Friends,

 

Can any let me know what is the maximum and the Minimum limit of the pressure gauge that can be used for testing , is there any code governing this

 

Thanks and Regards,

Bathula Anil Kumar

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...