Dear Srinivas,
 
Atleast 70% from thickness of the meterial, Exam: if 10 mm thk mean atleast 7 mm.
 
Regards,
Moorthy.

On 7 June 2010 09:32, Srinivas Engr <srinivas.gmsrini@gmail.com> wrote:
Dear All

What is the minimum fillet weld throat thickness requirement.?

For example Base material thickness is 10mm, for fillet weld, How
much  throat thickness is required?
pl explain...

Thanks
Srinivas

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...