Re: [MW:5437] Need P No list

Hi,
 
Please check ASME Sec. IX - QW/QB 422
 
Regards,
Moorthy,

On 7 June 2010 15:40, Muhammed Ibrahim PK <ibratech@gmail.com> wrote:
Hi,
 
You can get the P number list from ASME Sec. IX

Thanks & Regards
Muhammed Ibrahim PK



On 7 June 2010 09:39, nandu karande <nandukarande@gmail.com> wrote:
Dear all,
 i need P no List of Material,
if any one haveing this please forword this to me.

--
Nandkishor Karande
Welding Technology cell,
R&D, Product engg dept,
BEML KGF.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...