Monday, June 7, 2010

Re: [MW:5433] PWHT Procedure

This material (API 5L X52 Sch XXS (WT 12.7mm) does not require any PWHT.
As per B31.8/ B 31.4, the maximum wall thickness can be welded with out PWHT
is 1.25" (with a qualified Procedure).
Regards,,
sanjeevan GPS
----- Original Message -----
From: "Paul" <paulrapidheat@hotmail.co.uk>
To: "Materials & Welding" <materials-welding@googlegroups.com>
Sent: Monday, June 07, 2010 11:58 AM
Subject: [MW:5424] PWHT Procedure


> Dear all
> I have been asked to provide a procedure for heat treatment for
> following material by client can anyone help and please as i do not
> have a copy of the standard.
>
>
> PWHT required for Well Head Fecilities contract.
>
> The contract Code is ANSI B 31.8 Class 2Material ALI 5L Gr X52 SCH XXS
> Diamter 8 Inch and 6 Inch
>
> Looking forward for your feedback in this regard
>
> Paul Graham
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...