[MW:5388] Shell spec .weld requirement

Dear all

what is the welding requirement in shell spec DEP 31.38.01.31 for shop fabrication, is as per this spec TIG for root weld is compulsary ?

Regards

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step