Friday, June 4, 2010

Re: [MW:5388] Hardness requirement for P1 material

Dear Prasad,
 
But I remember 275HV10 for Cap and 250HV10 for others as per NACE MR0175.

J.GERALD JAYAKUMAR
00919344954677
 


--- On Thu, 6/3/10, N VENKATESWARA PRASAD <weldengr.velosi@gmail.com> wrote:

From: N VENKATESWARA PRASAD <weldengr.velosi@gmail.com>
Subject: Re: [MW:5371] Hardness requirement for P1 material
To: materials-welding@googlegroups.com
Date: Thursday, June 3, 2010, 5:24 AM

Dear Mr. Dharmesh,
 
As per NACE MR 0175 specification the pipes used in sour service shall have hardness less than 248Hv after welding.  It is applicable for base materials also.
 
Regards
 
N.V. PRASAD
WEDLING ENGINEER
VELOSI CERTIFICATION
QATAR

On Wed, Jun 2, 2010 at 11:26 AM, Dharmesh Mistry <Dharmesh.Mistry@heurtey.in> wrote:

Dear all,

 

Please let me know where I can find hardness requirement for P1 materials.

 

Thanks & Regards,

DHARMESH MISTRY

Direct : +91 22 6774 0074

Cell +91 98207 35814

Dharmesh.Mistry@heurtey.in

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...