Re: [MW:4507] ASTM A216 Vs ASME SA216 Difference

Hi, there is not diff. between boths only A and SA, the standart is iqual, review in ASME Section 2 and ASTM.
 
Agustin


De: vijay frnds <frndstovijay@gmail.com>
Para: materials-welding@googlegroups.com
Enviado: mar, marzo 9, 2010 4:42:51 AM
Asunto: [MW:4502] ASTM A216 Vs ASME SA216 Difference

Dear friends,


I have received the customer order for pipeline valves with ASME SA216 Gr WCB.

My doubt is there any diff. between ASTM A216 Gr WCB Vs ASME SA216 Gr WCB.

Thank you,


--
Urs . . .
Muthu
Smile make(s)miles ! ! !
Please don't print this e-mail unless you really need to! - this will preserve trees on our planet earth.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



¡Obtén la mejor experiencia en la web!
Descarga gratis el nuevo Internet Explorer 8
http://downloads.yahoo.com/ieak8/?l=e1

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...