[MW:4506] Re: depth of root concavity

Dear Chaitanya Purohit
thank you for reply.
your answer is coorrect. but in refered paragraph ,AWS says the weld
shall be flush with face of base metal.
regards

On Mar 9, 2:18 pm, Chaitanya Purohit <chaitanya_puro...@yahoo.co.in>
wrote:
> Dear Asghari
>
> Obviously its including reinforcement.
>
> Just draw the sketch and remove the reinforcement. Then draw the
> concavity......
>
> From the sketch you will come to know that there is no possibility to get
> the thickness equal to basemetal if you remove the reinforcement.....
>
> Regards.
> CK
>
> On 9 March 2010 11:06, Ali Asghari <asghari...@rocketmail.com> wrote:
>
>
>
> > Dear All
> > according AWS D1.1(4.8.1.4),the max depth of root concavity in PQR test
> > piece, is 2mm provided the total thickness of weld is equal or greater than
> > base metal.
> > now the total thickness of weld included reinforcment in face or not?
> > regards- Hide quoted text -
>
> - Show quoted text -

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35725] Dismillar material Welding

Dear experts,  In my Hydro Electric Project  materials using A517Gr.F and A537CL-II.  For A517Gr.F using E 11018M and A537CL-II using E 9018...