Hi Uzzmaan

You better read the following specifications in ASME Sec II Part C :
1) SFA 5.6 - Covered copper and copper alloy arc welding electrodes, 2) SFA:5.7 - Copper and Copper Alloy bare welding rods /electrodes, 3) SFA 5.15- Welding electrodes and rods for Cast iron.

You will get your answers.

If you still have any doubts then post your queries which will be answered immediately..

Regards

Prem Nautiyal
Mumbai.
Cell: 9820313278

On Tue, 09 Mar 2010 08:45:26 +0530 wrote
>Hey Guys how r u?

I m Uzzmaan and I hv recently joined this group. Can any body tell me

that what is the criteria to select the SMAW electrode to join cast

Iron, Brasses & Bronzes? I mean what is the criteria to select the

electrode that will join Brass or that can be used to fill the

porosities present in the cast iron,brass or bronze castings?



--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



PREM S NAUTIYAL
CELL : 9820313278

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...