Hi Nandesh,
                    For PWHT requirement detail is not given in ASME Sec IX, it is required based on construction code and Client specification.
 
As per ASME B31.3 , generally PWHT  required  for A333 Gr.6 is above 20 mm thk, but based on service fluid it will be higher requirement than code.
 
In my previous shell project some services requirement is 100%.
 
Louis
Singapore
 
 
--- On Tue, 26/1/10, Nandesh Kumar <nandeshkumar@rocketmail.com> wrote:

From: Nandesh Kumar <nandeshkumar@rocketmail.com>
Subject: [MW:4150] ASME SEC IX...PWHT?
To: materials-welding@googlegroups.com
Date: Tuesday, 26 January, 2010, 3:03 PM

Dear All,
 
For our LNG piping project, as per ASME SEC IX for a pipe 16 inch OD and Thk 21.44 mm PWHT is manadtory? We are welding root and hot pass TIG and others SMAW.
Material is ASTM A333 .
 
Thaks in advance
Nandesh Kumar A


Your Mail works best with the New Yahoo Optimized IE8. Get it NOW!.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


The INTERNET now has a personality. YOURS! See your Yahoo! Homepage.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...