Re: [MW:4126] Preparation of WPS

Yes,
 
The WPS can be prepared . However as the material is not included in QW 422 so the WPS will be  specific to material grade used in procedure qualification.
 
amarjit Singh
TEMA INDIA LTD
 
On 1/21/10, GOPU NAIR <gopunair5343@yahoo.com> wrote:
Dear All
 
Recently I have qualified a WPS on 20mm thick plate of EN10025 S355J2G3 using GTAW for root pass and SMAW for subsequent passes in accordance with Lloyds Register Rule for ship building.  The test piece has undergone Tansverse tensile test (2), Side bends (4) Impact test (3 Sets)  at centre of the weld, fusionline and HAZ at -20deg.C, Macro and Hardness (1). PT and RT were carried out the test samples prior to drawing the destructive test samples.  all the tests are passed with the required values. Record of welding for each run is prepared and maintained.
 
consumable used are ER70-S2 and E-7018-1
Plate material properties are: Yield 357 N/MM2, UTS 541 N/MM2, El;  30% IMPACT at -20deg C; 53min, 81 Av.
C;0.18, Si: 0.35 Mn ;1.4, P    ;0.015, S : 0.002 Ce; 0.428
 
PQR as per the Lloyds rules is under preparation.
 
My question is whether I can prepare a WPS and PQR in accordance with ASME Sec. IX using the above records.
 
Regards
 
Gopu/CEPL
 
 
 


The INTERNET now has a personality. YOURS! See your Yahoo! Homepage.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.




--
Amarjit Singh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...